Scientists from the Institute of Metallurgical and Material Studies. AA Baikova Ras and Chemistry Institute “Komi Science Center of the Ural Branch of the Russian Academy of Sciences” created solid solutions (Ti₁₋ₓzrₓ) with a zirconium content of 10% and 15%.

The tests have shown that zirconium addition increases hardness between 3.9 to 6.8 GPA and bending strength between 314 to 487 MPa at room temperature. It is important that alloy ceramics keep ductility for longer heating -a 15% zirconium sample protects 64% of the power even at 1600 ° C

New ceramics exceed ordinary maximum fractions in mechanical properties at temperatures above 1200 ° C.

Researchers say that Ti₃sic₂ Zirconia alloy has caused high -temperature materials for the energy, transportation, aviation and defense industry.

Source: Ferra

Previous articleThe scientists of the Russian Federation found how to improve the reproductive health of the cows – probiotics and technology 11 August 2025, 16:55
Next articleGazprom Neft experienced a new drilling technology in Russia on August 1925, 17:03
I am a professional journalist and content creator with extensive experience writing for news websites. I currently work as an author at Gadget Onus, where I specialize in covering hot news topics. My written pieces have been published on some of the biggest media outlets around the world, including The Guardian and BBC News.

LEAVE A REPLY

Please enter your comment!
Please enter your name here